Flexible rock wool blanket to 650 °C for tanks, large ducts and equipment. A1 non-combustible.
Wire-mesh faced blanket for large tanks and vessels with mechanically fixed lining.
Features galvanized wire mesh reinforcement sewn to rock wool blanket for mechanical strength and secure fastening to large surfaces, tanks, and vessels where mechanical fixing is required.
Rock wool wired blanket is a flexible rock wool mat faced with galvanised or stainless-steel wire mesh, giving it the mechanical retention needed for vertical surfaces, high-velocity ducts and equipment that sees vibration or airflow erosion.
| Property | Value |
|---|---|
| Maximum service temperature | up to 650°C (continuous) |
| Density | 100–140 kg/m³ |
| Thermal conductivity | 0.036–0.042 W/(m·K) at 25°C mean |
| Standard thickness | 25–100 mm |
| Standard dimensions | rolls 600 / 1200 mm wide × up to 5000 mm long |
| Fire classification | A1 (non-combustible, EN 13501-1 / Euroclass A1) |
| Composition | basaltic rock melted above 1500°C and spun into mineral fibres; organic binder 2–5% by weight |
| Standards | EN 13162, ASTM C612 (Type IV, up to 650°C) |
Wrap the blanket over the surface and secure with the integrated wire mesh using tying wire, bands or stud welding pins. Overlap joints by one mesh cell and weatherproof exposed outdoor runs with metal jacketing.
Manufactured to EN 13162, ASTM C612 (Type IV, up to 650°C) and controlled under a documented quality system. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.
Combines stable high-temperature performance with straightforward on-site fabrication. The material is asbestos-free, chemically stable in neutral and oxidising atmospheres, and supplied with full technical data sheets to support specification and inspection. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.
Rosetexwool is a rock wool wired blanket manufacturer and supplier serving more than 60 countries since 1982. Every rock wool wired blanket is produced under a documented quality system certified to ISO 9001, CE and SGS, with batch-level traceability from raw material to finished product.
What our manufacturing capability covers:
For quotations, lead times or technical data sheets, contact our team with your specification and target service temperature. Explore the Rock Wool insulation hub for the full range, or read the rock wool insulation selection guide for selection support.
rock wool strips — Narrow stone wool strips cut to precise dimensions for joints, gaps and perimeter fire barriers where full boards will not fit.
rockwool insulation board — Rigid basalt stone wool slabs, Class A1 non-combustible, water repellent and sound absorbing, with the compressive strength exterior wall systems require.
ceramic fiber special shaped — Vacuum-formed shapes produced to your drawing, so burner blocks, ladle covers and complex furnace geometries arrive ready to fit.
For the full stone wool range, temperature limits and density options, see our rockwool insulation guide.
For adjacent material options across temperature and application ranges, explore our ceramic fiber insulation hub.
For the wider selection logic behind this product, see the rock wool raw materials and manufacturing process.
Part of the Rock Wool product family.
Last updated: November 6, 2026
Rock wool insulation can withstand temperatures up to 650 °C for standard grades. It is classified as a non-combustible material (Euroclass A1, ASTM E84 Class A), making it ideal for structural fire protection, industrial pipe insulation, and building envelope applications.
No. Our rock wool products feature hydrophobic treatment with water repellency exceeding 98%. Unlike some insulation materials, rock wool maintains its thermal performance even in high-humidity environments. This makes it particularly suitable for outdoor pipework and marine applications.
Yes. Rock wool is manufactured from volcanic basalt rock — an abundant natural resource. It contains up to 75% recycled content, is fully recyclable at end of life, and contributes to building energy efficiency by reducing heat loss. It is RoHS and REACH compliant.
The optimal density depends on your application: 60–80 kg/m³ for general thermal insulation of tanks and vessels, 80–120 kg/m³ for pipe insulation and HVAC ductwork, 100–150 kg/m³ for load-bearing or structural applications, and 150+ kg/m³ for high-compression industrial flooring and sandwich panels.
Still deciding? Send your specs — we'll quote within 24 hours.
Get pricing
Fill out the form below with your requirements — our team responds within one business day.
Free sample + 24-hour engineering quote
Spec-match guarantee
Flexible rock wool blanket to 650 °C for tanks, large ducts and equipment. A1 non-combustible.
Basalt board to 650 °C. Fire-safe, water-repellent, for walls, roofs and oven casings.
High-density rock wool panels for sound absorption in plant rooms, halls and enclosures.