Rockwool Pipe Insulation for Steam Pipes
Pre-formed sections to 650 °C, Class A1, for steam, condensate and HVAC pipework.
Rock wool blanket faced with glass fiber mesh for extra surface strength on tanks and ducts.
rock wool blanket with glass fiber mesh facing providing improved surface durability, handling strength, and a smoother finish for industrial and building insulation applications where surface reinforcement is beneficial.
This rock wool blanket carries a glass-fibre mesh on one or both faces, adding surface abuse-resistance and easier handling while keeping the thermal and fire performance of standard stone-wool mat.
| Property | Value |
|---|---|
| Maximum service temperature | up to 650°C (continuous) |
| Density | 80–140 kg/m³ |
| Thermal conductivity | 0.036–0.042 W/(m·K) at 25°C mean |
| Standard thickness | 25–100 mm |
| Standard dimensions | rolls 600 / 1200 mm wide × up to 5000 mm long |
| Fire classification | A1 (non-combustible, EN 13501-1 / Euroclass A1) |
| Composition | basaltic rock melted above 1500°C and spun into mineral fibres; organic binder 2–5% by weight |
| Standards | EN 13162, ASTM C612 (Type IV, up to 650°C) |
Position the mesh-faced side outwards, secure with bands, pins or mesh ties, and butt seams tightly. Protect outdoor installations with a suitable weather jacket.
Manufactured to EN 13162, ASTM C612 (Type IV, up to 650°C) and controlled under a documented quality system. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.
Combines stable high-temperature performance with straightforward on-site fabrication. The material is asbestos-free, chemically stable in neutral and oxidising atmospheres, and supplied with full technical data sheets to support specification and inspection. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.
Rosetexwool is a rock wool blanket with glass fibre mesh manufacturer and supplier serving more than 60 countries since 1982. Every rock wool blanket with glass fibre mesh is produced under a documented quality system certified to ISO 9001, CE and SGS, with batch-level traceability from raw material to finished product.
What our manufacturing capability covers:
For quotations, lead times or technical data sheets, contact our team with your specification and target service temperature. Explore the Rock Wool insulation hub for the full range, or read the rock wool insulation selection guide for selection support.
rockwool wired blanket — Class A1 non-combustible and suited to big flat or curved areas where the insulation has to stay put under its own weight.
stone wool blanket insulation — Class A1 non-combustible and water repellent, it handles large-area coverage without the seams that create thermal bridges.
ceramic fiber plus blanket — An upgraded blanket with lower shot content and improved tensile strength, aimed at linings where consistency matters more than price.
For the full stone wool range, temperature limits and density options, see our rockwool insulation guide.
For adjacent material options across temperature and application ranges, explore our ceramic fiber insulation hub.
For the wider selection logic behind this product, see the external wall rock wool installation guide.
Part of the Rock Wool product family.
Last updated: November 6, 2026
Rock wool insulation can withstand temperatures up to 650 °C for standard grades. It is classified as a non-combustible material (Euroclass A1, ASTM E84 Class A), making it ideal for structural fire protection, industrial pipe insulation, and building envelope applications.
No. Our rock wool products feature hydrophobic treatment with water repellency exceeding 98%. Unlike some insulation materials, rock wool maintains its thermal performance even in high-humidity environments. This makes it particularly suitable for outdoor pipework and marine applications.
Yes. Rock wool is manufactured from volcanic basalt rock — an abundant natural resource. It contains up to 75% recycled content, is fully recyclable at end of life, and contributes to building energy efficiency by reducing heat loss. It is RoHS and REACH compliant.
The optimal density depends on your application: 60–80 kg/m³ for general thermal insulation of tanks and vessels, 80–120 kg/m³ for pipe insulation and HVAC ductwork, 100–150 kg/m³ for load-bearing or structural applications, and 150+ kg/m³ for high-compression industrial flooring and sandwich panels.
Still deciding? Send your specs — we'll quote within 24 hours.
Get pricing
Fill out the form below with your requirements — our team responds within one business day.
Free sample + 24-hour engineering quote
Spec-match guarantee
Pre-formed sections to 650 °C, Class A1, for steam, condensate and HVAC pipework.
Narrow strips for gap filling, joint sealing and irregular cavities in ovens and panels.
Wire-mesh faced blanket for large tanks and vessels with mechanically fixed lining.