Composite Silicate Plate
Flexible rare-earth silicate plate to 600 °C for curved and irregular surfaces.
Pre-formed pipe sections to 1100 °C for steam and process piping. Asbestos-free.
Pre-formed calcium silicate pipe insulation providing uniform and efficient thermal insulation for industrial piping systems. Same high-temperature resistance and low thermal conductivity as the board form, optimized for pipe applications.
Calcium silicate pipe insulation is supplied as pre-formed half-shells that snap around industrial piping, giving uniform, efficient thermal insulation with very low conductivity and a non-combustible A1 profile.
| Property | Value |
|---|---|
| Maximum service temperature | up to 650°C (ASTM C533 Type I; high-temp grade to ~1000°C) |
| Density | 170–250 kg/m³ (Type I) |
| Thermal conductivity | ≤0.065 W/(m·K) at 100°C; ≤0.095 W/(m·K) at 400°C |
| Standard thickness | 25–100 mm |
| Standard dimensions | pre-formed half-shells, pipe OD 15–1000 mm+ |
| Fire classification | A1 (non-combustible, EN 13501-1) |
| Composition | xonotlite calcium silicate hydrate reinforced with inorganic fibre; 100% asbestos-free |
| Standards | ASTM C533, EN 14306 |
Fit the half-shells around the pipe with joints staggered between layers and secure with stainless bands (316 grade for coastal/outdoor). Seal butt joints and apply aluminium jacketing on weather-exposed runs.
Manufactured to ASTM C533, EN 14306 and controlled under a documented quality system. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.
Combines stable high-temperature performance with straightforward on-site fabrication. The material is asbestos-free, chemically stable in neutral and oxidising atmospheres, and supplied with full technical data sheets to support specification and inspection. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.
Rosetexwool is a calcium silicate pipe insulation manufacturer and supplier serving more than 60 countries since 1982. Every calcium silicate pipe insulation is produced under a documented quality system certified to ISO 9001, CE and SGS, with batch-level traceability from raw material to finished product.
What our manufacturing capability covers:
For quotations, lead times or technical data sheets, contact our team with your specification and target service temperature. Explore the calcium silicate insulation hub for the full range, or read the calcium silicate insulation buying guide for selection support.
calcium silicate insulation board — Rigid calsil board carrying the highest compressive strength of any hard insulation block, holding its shape without deformation at working temperature while staying fully asbestos-free.
high density calcium silicate board — Ultra-high density board above 500 kg/m³ for applications where the insulation also has to carry mechanical load.
nano insulation board — Microporous board with exceptional thermal performance in an ultra-thin rigid profile, stable over long service at temperature.
For the full calcium silicate range, temperature limits and strength data, see our calcium silicate insulation guide.
For adjacent material options across temperature and application ranges, explore our rock wool insulation hub.
For the wider selection logic behind this product, see the what calcium silicate insulation is.
Part of the Calcium Silicate product family.
Last updated: November 6, 2026
Calcium silicate insulation boards can withstand continuous temperatures up to 1100°C. They offer high compressive strength and excellent dimensional stability, making them ideal for high-temperature pipe supports, furnace backup insulation, and aluminium smelter applications.
Calcium silicate offers significantly higher compressive strength (up to 6 MPa) than ceramic fiber blankets, making it the preferred choice for load-bearing insulation. It is supplied in rigid board form, easy to cut and machine. Ceramic fiber, however, offers higher temperature limits (up to 1430°C) and lower thermal conductivity in blanket form.
Absolutely. All our calcium silicate products are manufactured using an asbestos-free formula. They meet international health and safety standards including ASTM C533 and EN 14306, and are certified as non-hazardous material for transport and handling.
Still deciding? Send your specs — we'll quote within 24 hours.
Get pricing
Fill out the form below with your requirements — our team responds within one business day.
Free sample + 24-hour engineering quote
Spec-match guarantee
Flexible rare-earth silicate plate to 600 °C for curved and irregular surfaces.
Calcium silicate board above 500 kg/m³ where the lining carries load or takes abrasion.
Rigid calsil board to 1100 °C for furnace and kiln linings. High compressive strength.