Rosetexwool  Insulation Refractory Co., Ltd.
Ceramic Fiber Modules
Ceramic Fiber

Ceramic Fiber Modules

Pre-compressed folded modules for furnace walls. Faster to install than blanket, lower heat storage.

Density
160-260 kg/m³
Size
300/600×300×200-350 mm
Packing
Plastic bag + Carton/Pallet

Overview

  • Faster temperature cycling
  • Lower heat storage
  • Lower fuel costs
  • Increased productivity

Made from ceramic fiber acupuncture blanket, processed in dedicated machines. Folded modules are directly fixed to industrial furnace shell plates by various anchorages.

What Is Ceramic Fiber Modules?

Ceramic fiber modules are pre-compressed folded blankets anchored to a metal backing, enabling fast, uniform furnace-wall lining with low heat storage and rapid heat-up/cool-down.

Key Technical Specifications

Property Value
Maximum service temperature classification 1260–1430°C; service up to 1100–1250°C
Density 192–320 kg/m³ (as module)
Thermal conductivity ≤0.153 W/(m·K) at 500°C mean
Standard thickness 150–300 mm (module depth)
Standard dimensions 300×300 mm typical face; custom
Fire classification Non-combustible (ceramic fibre, asbestos-free)
Composition high-purity alumino-silicate (Al₂O₃ + SiO₂) blown fibre, no organic binder
Standards ASTM C892, ASTM C1086, ISO 10635, EN 10964

Properties & Advantages

  • Rapid, uniform furnace lining
  • Low heat storage — fast cycles
  • Anchor options for new or worn linings
  • Good thermal-shock resistance
  • Reduced installation time vs brick

Typical Applications

  • Industrial furnace and kiln walls
  • Heater and reformer linings
  • Annealing and heat-treat furnaces
  • Retrofit of worn refractory linings

Installation & Handling

Fix modules to the shell with the specified anchors (welded stud, threaded or marshal). Butt module faces tightly so the hot face is continuous; stagger rows to avoid through-joints.

Standards & Compliance

Manufactured to ASTM C892, ASTM C1086, ISO 10635, EN 10964 and controlled under a documented quality system. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.

Why Specify This Product

Combines stable high-temperature performance with straightforward on-site fabrication. The material is asbestos-free, chemically stable in neutral and oxidising atmospheres, and supplied with full technical data sheets to support specification and inspection. Supplied by a manufacturer holding ISO 9001, CE and SGS certifications, exporting high-temperature insulation to 60+ countries since 1982.

Manufacturer & Supplier

Rosetexwool is a ceramic fiber modules manufacturer and supplier serving more than 60 countries since 1982. Every ceramic fiber modules is produced under a documented quality system certified to ISO 9001, CE and SGS, with batch-level traceability from raw material to finished product.

What our manufacturing capability covers:

  • In-house melting, fibre-forming and finishing lines for consistent grade and density
  • Dimensional, density and thermal checks against ASTM C892, ASTM C1086, EN 10964
  • Asbestos-free, low-impurity formulations verified by incoming and outgoing inspection
  • Standard and custom sizes, OEM/ODM grades, and cut-to-size supply for project quantities

For quotations, lead times or technical data sheets, contact our team with your specification and target service temperature. Explore the ceramic fiber insulation hub for the full range, or read the ceramic fiber insulation buying guide for selection support.

Related Ceramic Fiber Products & Alternatives

ceramic fiber rope — Twisted refractory rope to 1260 °C for door seals, flange gasketing and expansion joint packing that has to stay compressible at heat.

ceramic fiber board alternative — A cost-effective board made from rare earth cotton for medium-temperature work to 600 °C where full refractory grade would be over-specification.

rock wool strips — Narrow stone wool strips cut to precise dimensions for joints, gaps and perimeter fire barriers where full boards will not fit.

For the full ceramic fiber range, temperature grades and density options, see our ceramic fiber insulation guide.

For adjacent material options across temperature and application ranges, explore our rock wool insulation hub.

For boiler and furnace back-up linings in power stations, see our power generation application page.

Part of the Ceramic Fiber product family.

Key features

  • Faster temperature cycling
  • Lower heat storage
  • Lower fuel costs
  • Increased productivity
  • Easy to install
  • Easy repairs
  • Thermal shock resistance

Typical applications

  • High-temperature reactors
  • Power generation turbines
  • Industrial furnaces

Technical specs

Density
160-260 kg/m³
Size
300/600×300×200-350 mm
Packing
Plastic bag + Carton/Pallet

Specifications

Parameter STD ModuleHP ModuleHZ Module
Class. Temp. 1260℃1260℃1430℃
Working Temp. 1050℃1100℃1350℃
Density (kg/m³) 160-260160-260160-260
Al₂O₃ (%) ≥44≥45≥34
ZrO₂ (%) ——≥15

Which grade should I choose?

Different grades are designed for different operating temperatures and environments. Use the comparison below to select the right grade for your application.

STD Module

1050℃

Al₂O₃: ≥44%

Standard industrial furnaces, boilers, backup insulation

Best for general industrial furnace insulation

HP Module

1100℃

Al₂O₃: ≥45%

Standard industrial furnaces, boilers, backup insulation

Best for high-temperature continuous operation

HZ Module

1350℃

Al₂O₃: ≥34%

Ultra-high temperature furnaces, glass kilns, ceramic firing

Best for industries requiring maximum thermal stability

Last updated: November 6, 2026

Frequently asked

What temperature can ceramic fiber insulation withstand?

Ceramic fiber insulation withstands temperatures from 1100°C to 1430°C, depending on the grade. Standard (ST) and High-Purity (HP) grades are rated for 1260°C, while High-Alumina (HA) handles 1360°C and Zirconia (HZ) reaches 1430°C. Always match the grade to your specific operating temperature.

What are the differences between COM, ST, HP, HA, and HZ grades?

The grades differ mainly in alumina (Al₂O₃) content and temperature rating. COM (1100°C) is the economy grade. ST (1260°C) is the standard industrial grade. HP (1260°C) offers higher purity with lower shot content. HA (1360°C) has higher alumina for superior thermal stability. HZ (1430°C) contains zirconia for the highest temperature resistance.

Is ceramic fiber insulation safe?

Yes. Our ceramic fiber products are 100% asbestos-free and manufactured to international safety standards. They are classified as non-carcinogenic under EU Directive 97/69/EC. We recommend standard PPE (gloves, dust mask) during handling, as with any fibrous insulation material.

How is ceramic fiber blanket installed?

Ceramic fiber blanket can be cut to size with a utility knife and secured using high-temperature anchors, pins, or stud welding. For furnace linings, a layered installation is recommended. For pipe insulation, wrap and secure with stainless steel bands. Full installation guidance and technical support are provided with every order.

What are the typical applications for ceramic fiber products?

Ceramic fiber is widely used in industrial furnaces, kilns, boilers, petrochemical heaters, power generation equipment, incinerators, and building fire protection systems. It is ideal for backup insulation, expansion joints, door seals, and high-temperature gaskets.

Still deciding? Send your specs — we'll quote within 24 hours.

Get pricing

Request a quote for Ceramic Fiber Modules

Fill out the form below with your requirements — our team responds within one business day.

Free sample + 24-hour engineering quote

  • Free cut-to-size samples for lab testing or plant trial, shipped by courier.
  • Material recommendation, drawings and an FOB or CIF price within one working day.

Spec-match guarantee

  • Every batch tested against the MTC and TDS that ship with your order.
  • Off-spec material: we re-ship or refund in full, freight both ways on us.
or email us directly

You may also like

Request a Quote WhatsApp

Get in touch

Free consultation & tailored quotation

Request a Quote WhatsApp